Thank you MarlaMike.
But the doubt is if the 32" size Blind Flange and 32" Welding Neck flange 300lb have the same hot working and reduction as to consent to take sampling for mech. test. from unique test blank.
 
Thank you MarlaMike.
But the doubt is if the 32" size Blind Flange and 32" Welding Neck flange 300lb have the same hot working and reduction as to consent to take sampling for mech. test. from unique test blank.