I have an application in which we need to connect an aluminium plate to a aluminium block using two bolts. There could be a fair amount of wind load at this joint so it must be fairly strong and it is also located in a coastal salt water area.
The plan was to use hot dipped galvanized hardware to help with corrosion, as they have long proven history. The down fall is that the added thickness of zinc coating requires oversized threads tapped in the aluminium block. This is problem as we do not have the correct oversized tap and would have to get one custom made.
I have looked at various other bolt coatings claiming high corrosion resistant, i.e. Geomet, Dacromet, Ultra Corrosion Resistant etc. All of these have displayed images of 1000 hour salt spray tests indicating they far out perform hot dipped galvanized. I would have taken this to be true except I came across another source that indicated salt spray tests weren't necessary true indications of real world performance.
It's hard to argue with the few hundred years history of hot dipped galvanized. So my question then, is a salt spray test a true indication of real world performance for corrosion protection?
The plan was to use hot dipped galvanized hardware to help with corrosion, as they have long proven history. The down fall is that the added thickness of zinc coating requires oversized threads tapped in the aluminium block. This is problem as we do not have the correct oversized tap and would have to get one custom made.
I have looked at various other bolt coatings claiming high corrosion resistant, i.e. Geomet, Dacromet, Ultra Corrosion Resistant etc. All of these have displayed images of 1000 hour salt spray tests indicating they far out perform hot dipped galvanized. I would have taken this to be true except I came across another source that indicated salt spray tests weren't necessary true indications of real world performance.
It's hard to argue with the few hundred years history of hot dipped galvanized. So my question then, is a salt spray test a true indication of real world performance for corrosion protection?