I'm looking to establish testing qualification criteria for corrosion for wind turbines installed in coastal/offshore applications. Are there any standards that are commonly used across different industries?

Essentially, I would like to set my criteria as "withstand X hours under standard salt fog test conditions." Any recommendations? Where should I start looking?

-Adrian
 
ASTM. There are many specs on how to do the test and many material and coating specs that require it.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
NORSOK M-001 Materials selection

DNV Recommended Practice CORROSION PROTECTION OF SHIPS

DNV Corrosion & Materials Degradation

Hempel A/S CORROSION PROTECTION OF OFFSHORE STRUCTURES

UK Health & Safety Executive - Offshore oil & gas


Material Selection Corrosion Prevention Offshore Oil & Gas

Corrosion in offshore wind energy - 'a major issue'
 
Thanks for the references! Very helpful.
 
There's a salt fog test specification in MIL-STD-810, as well.

TTFN
faq731-376
7ofakss
 
Intermittent salt fogs have better correlation with most natural weathering than continuous (ASTM B117 type) salt fogs. In the real world, you typically have spray/dryoff/spray/dryoff/dew/dryoff, et cetera. The old B117 style salt fogs are a continuous wet condition.
 