Hello, I'm a metallurgical tech that recently took over the corrosion department at my lab and I have a chamber that is causing a lot of problems.

Before I transferred, we purchased a chamber for CASS testing per ISO 9227 and ASTM B368. To spare the drama of everything, we didn't end up with a chamber that could easily meet those specs.

Long story short, does any have experience with getting immersion heaters to work in these tests? Or do you think it would be possible to retrofit it with plate heaters from a QFog?

I really appreciate any help.
 