Does anyone know a good resource (publications, website, etc) that provides a comprehensive list of the polynomial equations for various conductors used in T&D? Trying to put together some in-house tools for sag-tension-creep determination for a project we have.

Thanks in advance for any input!
 
The makers of PLS-CADD mention that polynomial the models they supply came from publicly available sources.
 
The Aluminum Association has stress/strain graphs of various popular conductors and the polynomials you are looking for are on those graphs.

go to


and look for the stress strain creep curves for aluminum overhead electrical conductors at the bottom of the page.
 
The PLS CADD website has a big collection of wire files available for download. The wire files have the polynomial coefficients in them.
 