Aug 19, 2002 #1 metman Materials Joined Feb 18, 2002 Messages 1,187 Location US Is SAE S1420F Stainless Steel (AMS 5620) same as AISI 420F ? Jesus is The TRUTH
Aug 20, 2002 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US Yes, it is the alloy known by the UNS designation S42020. It is recognized in ASTM A 582 and A 895, in addition to SAE AMS 5620. Upvote 0 Downvote