Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations LittleInch on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SAE 950 Steel Spec

Status
Not open for further replies.

Craner

Automotive
Joined
Jan 20, 2006
Messages
11
Location
CA
Could somebody tell me the n & r values and UTS for, SAE 950
 
HUH? SAE950 is not a steel specification. 950 is a HSLA Strength grade, however usually n & r values are not specified for HSLA steels.
 
950 is the old designation according to SAE J1392. The new designation is 340 according to SAE J2340. The UTS is specified to be a minimum of 410 MPa. n-value is not a requirement of this standard, and its value will change with strain. The following presentation from US Steel shows some data for HSLA 340 steel:


The r-value will depend on whether it is cold-rolled or hot-rolled, but you can use r ~ 1 for an estimate.
 
Status
Not open for further replies.