Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

SAE 5160 1

Status
Not open for further replies.

DeanBMI

Mechanical
Oct 27, 2009
6
Anybody know where I could source some SAE 5160 flatbar. Preferably 1/2"x1" or 3/4"x1".

Where would I find a good reference for heat treating it?

Thanks
 
Replies continue below

Recommended for you

Heat Treater's Guide published by ASM International is a good reference for the heat treating of 5160.
 
Dean,

What quantity do you need? 1 foot? Enough to make 10000 parts that are 2 inches long? McMaster Carr probably stocks this for small quantities. Admiral Steel or Thompson Steel are possibilities for larger quantities.
 
McMaster Carr carries it if you're looking for just a small amount.
 
Yes, Mcmaster has it. What's this stuff like to work with? Can it be cut on a bandsaw?
 
I have cut it many times on a bandsaw.
 