I am dealing with AlCh3 and alot of my surrounding supplies, materials and my feed system is corroding. I was wondering if anyone out there knows of a company which can supply a sacrificial anodes to ensure the life cycle of at least my feed system.
Thanks
Sacrifical anodes-do you mean Magnesium sacrificial anodes.Try a net search under "hot water magnesium sacrifical anodes", or "mangesium producers". I know that these are produce as extruded bars in Norway and Canada
Zinc anodes are used to protect alu., iron, copper,
& brass on boats in salt water. They come in MANY
shapes & sizes. Many with threads for mounting.
Everything needs to be grounded/bonded for proper
protection. Good Luck!