I have designed a device which has an Inconel X750 spring within a large 316 SS body. The Inconel is passivated so its corrosion potential is -0.3, the 316 SS (active) has a potential of -0.79. The spring material is only 0.025" thick. The SS body is a piece of 1 1/2" thick bar stock with a hole drilled in it for the passage of various chemicals through the ball check spring mechanism. The idea is that the stainless body would become the sacrificial anode to preserve the spring. We also are planning on making the body out of HC-276 (potential -0.71)
Is this a good idea?