SA516 Gr.70 - classification as per ISO / TR 15608-2013

Status
Not open for further replies.

Emilio87

Petroleum
Mar 26, 2014
7
Hi,
The material SA/A516 Gr.70 in accordance with ISO / TR 15608-2013 is classified as Subgroup 1.1 or 1.2?

Thank you and regards,
Emilio A.

 
Replies continue below

Recommended for you

This material SA/A516 Gr.70 is in ISO/TR 15608:2005[1] group 11.1
 