I have storage tank made from SA516 gr 60 material. Tank covered by API 650. Please look at my inerpretation of impact testing energy value. It is important for me.
API 650 twelfth ed. 2013
SA516-60 in table 4.4b -> material group III or IIIA
Table 4.5a -> min value 20J
Thanks in advance for any help