Can we use SA36(bar)as anchor bolt instead of SA307B?

The tensile stress for SA36 is 58-60 ksi and yield stress is 36ksi while tensile stress for SA307B is 60Ksi and yield stress is not given any where!

Thanks for your input.

Hiren
 
Replies continue below

Recommended for you

mechmania;
Not using SA 307 Grade B material, but you can use SA 307 Grade C material in place of SA 36 for nonheaded anchor bolts, because the Grade C material can be produced to conform to the ASTM A 36 requirements, as stated in the ASME SA 307 specification under the Scope.
 