can the SA/GB6654 16MnR 6mm thickness plate be used in ASME viii div.1

the SA/GB 6654 16MnR thickness is more than 0.25in(>0.25in) in the ASME SEC.II PART D.
 
Replies continue below

Recommended for you

the 6mm thickness sa/gb 6654 16mnr plate is not in the ASME II PART D. someone say i can't use the 6mm thickness SA/GB 6654 Plate in ASME designing.
 
knstar:
I did a quick review of Section II part D and did not find this material specification and Grade. If it is not listed in Section II, Part D, it cannot be used for pressure boundary application. This material can be used as non-pressure boundary material under the rules of ASME B&PV Code, Section VIII, Div 1.
 
There is a limits of size/thickness for
16MnR in the ASME SEC.II PART D page 22 line 14.

This is a new material in the 2008 addenda for the sec. II PART D
 