Hello everybody.
I have steel SA-737 Gr.B
Nominal composition is C-Mn-Si-Cb. Well, I use table TM-1 from ASME BPVC Section II part d to know Moduli of Elasticity to use it in calculations.
What string shall I use? Material group A?
Thanks for advance!
 
Replies continue below

Recommended for you

Yes, this would be the closest material grouping.
 
Great!
But in Table 3-D.2M from ASME BPVC div.2 Section VIII it will be carbon steel the nearest group to determinate Ncss and Kcss? Yes?
Thank you for help!
 
The SA 732 material specification is low alloy because of the small addition of columbium, which results in a fine grained texture and increased strength to some extent. Overall, it is closest a microalloy carbon steel.
 