Mar 4, 2020 #1 Ramezadel Mechanical Joined Jul 7, 2019 Messages 11 Location EG good morning i am trying to weld SA 517 grade B and S690 QL1 using SMAW electorde 11018 M for repair for transpot LPG pressure vessel but every time PQR fails at charpy v notch impact test give me max reading 26 joule need for help please...
good morning i am trying to weld SA 517 grade B and S690 QL1 using SMAW electorde 11018 M for repair for transpot LPG pressure vessel but every time PQR fails at charpy v notch impact test give me max reading 26 joule need for help please...
Mar 4, 2020 #2 r6155 Mechanical Joined Jan 12, 2010 Messages 3,015 Location AR Plate S690 QL is for structural purpose, not for pressure vessels. As I say in your post of 17feb20, you need a welding engineer. Also contact a pressure vessel engineer. Regards Upvote 0 Downvote
Plate S690 QL is for structural purpose, not for pressure vessels. As I say in your post of 17feb20, you need a welding engineer. Also contact a pressure vessel engineer. Regards
Mar 5, 2020 Thread starter #3 Ramezadel Mechanical Joined Jul 7, 2019 Messages 11 Location EG i have pessure vessels head made from naxta 70 model 1980 that is why we decide to use it Upvote 0 Downvote
Mar 5, 2020 #4 r6155 Mechanical Joined Jan 12, 2010 Messages 3,015 Location AR This pressure vessel is very dangerous. I understand that you are not in a position to handle this issue. Are you aware of your responsibility? Regards Upvote 0 Downvote
This pressure vessel is very dangerous. I understand that you are not in a position to handle this issue. Are you aware of your responsibility? Regards