Hello Everyone,

I would like to ask the Minimum Design Metal Temperature allowed by ASME VIII Div.1 for SA 517 Gr.F material. I have read Part UHT and UCS to find some answers. Will UCS 66 apply to SA 517 and under what group?

Appreciate your comments.

 
Replies continue below

Recommended for you

napster385, I am not familiar with Part UHT, but SA-517 is listed in Table UHT-23, and presumably is bound by UHT-5 and UHT-6. Especially see UHT-5(c), which seems to require impact testing of these steels.

Regards,

Mike
 
Hi napster385,
Please refer to Table A1.15 of ASME SA-20.
Cheers,
gr2vessels
 