Is it permissable to bend SA-516 gr 70 plate for ASME code use with no further treatment? If not, where in the code could I locate that?
 
Replies continue below

Recommended for you

What is your application??
For plate used in unfired pressure vessels, please review ASME B&PV Code, Section VIII, Div 1, Part UCS-79.

For plate used in ASME Section I, boilers, there is no limitation.
 