Does any one have connections / leads on supply of metric (8mm & 10mm) SA-516 70N plate in the US/Canada?

We have a series of pv's that are for export and designs and client expectations are for metric material.

Any help would be greatly appreciated. We are in California if that matters :)

Jason
 
Replies continue below

Recommended for you

I don't know how much you are talking about, but, any mill can roll plate to any decimal thickness. you can order plate at .40" thickness and .48 thickness.
 
The first thing I'd do is call a plate supplier.
 
In addition to the above comments, the plate supplier/miller might require you for some tonnage if you want metric thicknesses.

-MechCiVAero