hi..

Mounded Bullet
DP = 17.5 barg
DT = -46 / 80 deg C

Based on the above design conditions I have selected MOC for Shell/Dish plate SA 350 LF3 and same is procured by vendor. Now client is not accepting this material because of Ni content of 3.5% as it is specified in the client specification that 3.5% Ni shall not be used and asking me to go with SA 350 LF2 cl.1.

Since the material has already been procured, client is asking me to give proper justification to take deviation to specification for using SA 350 LF3 instead of SA 350 F2 Cl.1 material.

Please let me know if any other information is required

kindly help me to solve this issue.

Thanks
 
This is a contract issue,and not a technical issue related to the Code. You need to work with the client to resolve it. Was there a PO or contract,which indicated acceptable materials of construction. Having puchased material without input from the client is now your responsibility.
 
arvindpandit said:
...as it is specified in the client specification that 3.5% Ni shall not be used

It's yours.

Regards,

Mike

The problem with sloppy work is that the supply FAR EXCEEDS the demand
 
Have sometimes wondered why materials such as 3.5% Ni and 9 % Ni steels have fallen out of favour in recent times for applications where lower design temp is < -40degC or so, if it is not corrosion resistance related.

What is the service fluid in this vessel - liquified anhydrous ammonia or propane ?
 
The contract is the contract and 350-LF2 will be able to comply with the service. The customer may well be applying the 1% Ni max requirement for H2S service, whether practical or impractical in this case.
 