Oct 26, 2010 #1 ijzer Materials Joined Oct 25, 2002 Messages 313 Location NL Material SA 350 LF2 is not accepted for pressure parts in ASME 1. Is it allowed to use this material in a B16.34 valve in an ASME 1 system?
Material SA 350 LF2 is not accepted for pressure parts in ASME 1. Is it allowed to use this material in a B16.34 valve in an ASME 1 system?
Oct 27, 2010 #2 reverman Mechanical Joined Jul 22, 2008 Messages 142 Location US A b16.34 valve can be made with LF2 but if the ASME code does not allow it then it won't meet the ASME 1. so the valve will meet B16.34 but not be allowed in use on a ASME 1 system would be my guess. Upvote 0 Downvote
A b16.34 valve can be made with LF2 but if the ASME code does not allow it then it won't meet the ASME 1. so the valve will meet B16.34 but not be allowed in use on a ASME 1 system would be my guess.