Hi All. I am going to weld a SA-213 T91 2" diameter .240" MWT tube to a boiler header SA-335 P12 13" diameter 3.5" MWT. I need to qualified a WPS and I am planning to use ER90S-B9 as the filler metal. Any recommendation about other filler metals that could be suitable for these materials?
 
Replies continue below

Recommended for you

ER90S-B3 is a better option? any pros and cons between those feller metals for my application?
 
I agree with weldstan, the ER90S-B3 would be my first choice for this dissimilar metal weld given the base materials.
 