if the the impact sample is subsize, and less than 80% of actual wall thk a reduction in temp is needed my quaestion is
Would the nominal wall be used for the calc or can the wall be measured.
If i use the nominal it less than 80% if i use the low end of the wall thickness its within.(is that stretching the intent of the code?)
But how do i know if the impact sample was at the right temp if i dont know what the pipe wall was measured.
Or do i use the sch nominal thickness.
Im not confident aBOUT THIS MANUFACTURER.
mdk
Would the nominal wall be used for the calc or can the wall be measured.
If i use the nominal it less than 80% if i use the low end of the wall thickness its within.(is that stretching the intent of the code?)
But how do i know if the impact sample was at the right temp if i dont know what the pipe wall was measured.
Or do i use the sch nominal thickness.
Im not confident aBOUT THIS MANUFACTURER.
mdk