May 19, 2021 #1 POPPASMURFF1942 Petroleum Joined Nov 2, 2006 Messages 11 Location US API-510 states if the material is unknown to use the allowable stress value for SA-283-C. Can't seem to find it
API-510 states if the material is unknown to use the allowable stress value for SA-283-C. Can't seem to find it
May 19, 2021 #2 Christine74 Mechanical Joined Oct 8, 2002 Messages 560 Location US What code was the vessel built to? If it was ASME Section VIII Division 1, the current edition of ASME Section II Part D lists the allowable stress for SA-283 Grade C plate as being 15.7 ksi for design temperatures up to an including 500F. -Christine Upvote 0 Downvote
What code was the vessel built to? If it was ASME Section VIII Division 1, the current edition of ASME Section II Part D lists the allowable stress for SA-283 Grade C plate as being 15.7 ksi for design temperatures up to an including 500F. -Christine
May 20, 2021 #3 Guest You will see SA-283 used in a lot of older vessels and storage tanks. It has been superseded by SA-516. "Everyone is entitled to their own opinions, but they are not entitled to their own facts." Upvote 0 Downvote
You will see SA-283 used in a lot of older vessels and storage tanks. It has been superseded by SA-516. "Everyone is entitled to their own opinions, but they are not entitled to their own facts."