A vessel is in hydrogen service.
The forging´s material is SA-266-Gr.2 Normalized with test in accordance to NACE-TM284 & NACE-TM0177.
Our supplier is ofering Quenched and Tempered instead of Normalized.
I wold like to know if there are advantages or disadventages using this material in Quenched and Tempered instead of Normalized heat treatment.

Tanks in advance.
 
Replies continue below

Recommended for you

Per ASME SA-266, you have several heat treatment options for this material; annealed, normalized, and normalized and tempered. If agreed upon between the purchaser and supplier, liquid quenched and tempered heat treatment can be supplied.

Normally, a liquid quench and temper heat treatment is required on material that is of a thickness or geometry to assure meeting thru thickness mechanical property requirements, where a normalization heat treatment may not achieve the required thru thickness mechanical properties.

Advantages of Q&T; a consistent, thru thickness structure that produces more uniform mechanical properties, and increased toughness.

Disadvantage; potential distortion concerns from liquid quenching, increased cost for this heat treatment and more care during welding fabrication to keep heat inputs from adversely affecting the quenched/tempered bulk material properties.
 