SA-266 GR.2 NOMINAL DESIGNATION

Status
Not open for further replies.

chrysa1975

Materials
Nov 14, 2007
64
SA-266 GR.2 is not included in ASME B16.34. However, please advise, if we needed to categorize it in a nominal designation just like in Table 1 of ASME B16.34, it could be C-Si or C-Mn-Si? What would be the P-T rating group that could match closer a flange made by this material?
 
Replies continue below

Recommended for you

Ok, I conclude to use C-Si designation and 1.1 material group considering that it is the alternative of the SA105.
If someone can verify or amend, is welcome.
 
You cannot categorize that into any head as than it won't be as per ASME B 16.34.

Very difficult to place ASTM A 266 under any head, but C-Mn-Si would be more stringent.

DHURJATI SEN