Specifically, S40910.

Question: The 'Other Elements' column has a formula:

Ti 6 x (C+N) min, 0.50 max; Cb 0.17

(I want to be sure I understand this formula completely.)

This formula means, with C = 0.030, N = 0.030,

Ti, min = 6 x (0.030+0.030) = 0.36%

Therefore, Ti content is 0.36-0.50%.

Am I correct?

--------------------------------
Fitter, happier, more productive
 
Right on. Thanks again!

--------------------------------