Hello Everyone,
As per ASME sec8 Div1 can we use SA194 fastners??
Thanks
 
Replies continue below

Recommended for you

c8829, refer to Sec II, Part D, Table 3. You may use SA-194 nuts with appropriate studs / bolts. SA-194 covers a wide range of metallurgies, as does, for example, SA-193 for studs.

SA-193 B7 / SA-194 2H very common.

Regards,

Mike
 
Thank Mike.
Table 3 of SEC.II part D not mention anything about SA 194, same with UCS-23.
"SA-193 B7 / SA-194 2H very common." I agree with you 100%
but I got comment from my client(germany) that "check availability of material as per SEC.II part D."
 
c8829, refer your client to UG-13, UCS-11.

Regards,

Mike
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor