Can someone provide me with S99 (C 0.36/0.44 Si 0.10/0.35 Mn 0.45/0.70 Cr 0.50/0.80 Mo 0.45/0.65 Ni 2.30/2.80) fatigue properties, preferable S-N.
 
Replies continue below

Recommended for you

I doubt that this exists in the public domain. You should contact Corus, as they are one of the only producers of this grade.
 