Nov 7, 2006 #1 vorwald Aerospace Joined May 25, 2001 Messages 94 Location US Can someone provide me with S99 (C 0.36/0.44 Si 0.10/0.35 Mn 0.45/0.70 Cr 0.50/0.80 Mo 0.45/0.65 Ni 2.30/2.80) fatigue properties, preferable S-N.
Can someone provide me with S99 (C 0.36/0.44 Si 0.10/0.35 Mn 0.45/0.70 Cr 0.50/0.80 Mo 0.45/0.65 Ni 2.30/2.80) fatigue properties, preferable S-N.
Nov 7, 2006 #2 TVP Materials Joined Apr 12, 2002 Messages 4,592 Location US I doubt that this exists in the public domain. You should contact Corus, as they are one of the only producers of this grade. Upvote 0 Downvote
I doubt that this exists in the public domain. You should contact Corus, as they are one of the only producers of this grade.