As for P,S values are more like
J0- P,S : 0,040 percent N : 0,015 ( all maximum )
J2- P,S : 0,035 " N : no
( for long products P and S may be 0,005 more ).
All those qunatities are actually very small, so you should estimate if they are a concern at all for your application
( most probably they are not - this quality being conventional
construction oriented. )