S2 Tool Steel is also call what?

Status
Not open for further replies.

petersi

Automotive
Feb 3, 2011
88
I know there are many names for the same steel in different countries. Is there any conversion chart? I want to what is S2 steel call in China. thanks
 
Replies continue below

Recommended for you

There are cross references of commercial names published.
One is an ASM book, another is Key to Steel which is a German publication.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Silicon Tool Steel (and shock resistant) , another designation is 310 (per mentioned ASM Tool book).
 
There is no direct equivalent of S2 (T41902) in any of the tool steel specifications in Stahlschl[ü]ssel.
 