Hi, I am trying to do some fatigue calculations on a component, but find that there are not enough material data (S-N data). So I am trying to generate my own data (mainly with higher stress ratios) to use in conjunction with those available. However, the data available are at a different heat treat condition. So my question is what sort of procedures is needed to correlate the data? Is it recommended to do such a correlation? Also, how many stress ratios should I replicate? Should I just replicate 1 stress ratio and assume all other stress ratio are related in the same manner? Are there any standards available for correlating S-N data?? Please give me some advices.
Thanks in advance.
Thanks in advance.