Looking for information / supplies for material type S-135.

Pipe Grade: S-135T
Min Yield Strength: 135,000
Max Yield Strength (psi): 165,000
Min Tensile Strength (psi): 145,000
Impact Energy ft-lb @ 75°F: 59 min
Hardness: 38 HRC max