Greetings -
We are working on rehabilitating an existing concrete water tank 24'L x 12'W x 10'H constructed in 1998. The tank appears to be in fairly good shape and the owner indicated no leakage prior to it being emptied in 2017.
We want to make sure the tank is OK for recommissioning so will use HLM 5000 on the interior wall. We will waterplug any problematic appearing areas on the interior prior to application of the HLM 5000.
Two Issues:
1. TANK COATING: The owner would like the exterior treated with HLM 5000 which I am hesitant to do as I don't believe it will actually improve the tank integrity, and may pose greater issues with future maintenance.
2. EVIDENCE OF CORROSION: In a few exterior locations along the wall faces there are "rust" streaks and the owner would like us to determine the cause prior to painting the tank's exterior wall. The owner's rep has requested that we chip out the concrete until we reach the source of the rust stains before we determine what restoration methods should be. Since the stains are streaks no more than 2' long and there are only 5 of them I am of the opinion that we leave well enough alone.
Would like your thoughts on the TANK COATING issue.
For the CORROSION issue are there good references which address similar scenarios?
Thank you.
We are working on rehabilitating an existing concrete water tank 24'L x 12'W x 10'H constructed in 1998. The tank appears to be in fairly good shape and the owner indicated no leakage prior to it being emptied in 2017.
We want to make sure the tank is OK for recommissioning so will use HLM 5000 on the interior wall. We will waterplug any problematic appearing areas on the interior prior to application of the HLM 5000.
Two Issues:
1. TANK COATING: The owner would like the exterior treated with HLM 5000 which I am hesitant to do as I don't believe it will actually improve the tank integrity, and may pose greater issues with future maintenance.
2. EVIDENCE OF CORROSION: In a few exterior locations along the wall faces there are "rust" streaks and the owner would like us to determine the cause prior to painting the tank's exterior wall. The owner's rep has requested that we chip out the concrete until we reach the source of the rust stains before we determine what restoration methods should be. Since the stains are streaks no more than 2' long and there are only 5 of them I am of the opinion that we leave well enough alone.
Would like your thoughts on the TANK COATING issue.
For the CORROSION issue are there good references which address similar scenarios?
Thank you.