Parts are made of SS 316L. We found about 1% of parts with brown marks, look like rust.
The OD surface go through grinding and cleaned with Alconox and Oakite 31, rinse with DI water.
What could be the cause? Is it from the material? A lab told us they found Manganese Sulfur inclusion in these areas. Does it make sense?
When parts come off our product line, we could not find anything like this. We can see some surface imperfections, rounded dots look rough and not as shiny as surrounding area. Our customer clean parts with Alconox and rinse with "soft water", then they found them. Does that mean our parts have something which could cause this?
Thank you for your help.
The OD surface go through grinding and cleaned with Alconox and Oakite 31, rinse with DI water.
What could be the cause? Is it from the material? A lab told us they found Manganese Sulfur inclusion in these areas. Does it make sense?
When parts come off our product line, we could not find anything like this. We can see some surface imperfections, rounded dots look rough and not as shiny as surrounding area. Our customer clean parts with Alconox and rinse with "soft water", then they found them. Does that mean our parts have something which could cause this?
Thank you for your help.