Guys,
Can you help i have a shaft with a dia in the middle greater than the shaft.
the drawing states one end of the shaft as datum A the other end as datum B.
the run out between datum A and B must be no more than 0.0005" the shaft is .3" in dia and 1.5" long.
one end and dia of the shaft are produced on a differant machine.
i then clamp this end in nice bored soft jaws and turn the other end.
my problem is when i locate the end i have just turned in a vee block put a dti on the other end and spin the part the run out reading is very good no more than 0.0003" however when i turn the part aroung locate the dia i didnt turn in the vee block and check again the reading is now 0.0015"???
both parts are round and straight i cant see where the error is coming from any advise? i cant turn the end in the same set up.
Can you help i have a shaft with a dia in the middle greater than the shaft.
the drawing states one end of the shaft as datum A the other end as datum B.
the run out between datum A and B must be no more than 0.0005" the shaft is .3" in dia and 1.5" long.
one end and dia of the shaft are produced on a differant machine.
i then clamp this end in nice bored soft jaws and turn the other end.
my problem is when i locate the end i have just turned in a vee block put a dti on the other end and spin the part the run out reading is very good no more than 0.0003" however when i turn the part aroung locate the dia i didnt turn in the vee block and check again the reading is now 0.0015"???
both parts are round and straight i cant see where the error is coming from any advise? i cant turn the end in the same set up.