Hi Everyone and Anyone,
Need some more advice, currently reviewing the process of rubber to metal bonding. Got the general idea but wondered if anyone knows of a good resource on the subject.
Product needs to be well bonded and samples I have received have been inconsistent (good bond, bad bond on same piece).
Items are compression moulded with an EPDM to various metals.
I believe the issue is primarily with the thickness of the undercoat, as the failures appear to be between the topcoat and the undercoat.
Any advice is welcome
Need some more advice, currently reviewing the process of rubber to metal bonding. Got the general idea but wondered if anyone knows of a good resource on the subject.
Product needs to be well bonded and samples I have received have been inconsistent (good bond, bad bond on same piece).
Items are compression moulded with an EPDM to various metals.
I believe the issue is primarily with the thickness of the undercoat, as the failures appear to be between the topcoat and the undercoat.
Any advice is welcome