rubber bellow/air spring crack/burse hole repair

Status
Not open for further replies.
If it were a patchable defect you'd need to apply the patch on the inside, but you can't.
 
My application only use the rubber with removable plates on both sides. So, I can access the inside.¡

R.Efendy
 
Check the condition of the rubber first.
If it is hard, brittle, or cracked then you need to replace the whole thing.
If it is a small hole less than a couple of mm and in a flat area, you might stand a chance.
But you need to know the cause before you even think about it.
Sounds like you have an external issue.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, consulting work welcomed
 