Jan 31, 2005 #1 homerphish Mechanical Joined Oct 7, 2003 Messages 48 Location US What does "RT / UT % per welder" mean in reference to welding? What do RT and UT stand for?
Jan 31, 2005 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US RT and UT refer to the following nondestructive test methods; Radiographic Testing (RT) Ultrasonic Testing (UT) The % refers to inspection coverage. Upvote 0 Downvote
RT and UT refer to the following nondestructive test methods; Radiographic Testing (RT) Ultrasonic Testing (UT) The % refers to inspection coverage.