Hi Folk!
Lets kill some confusion about the RT requirement in accordance with ASME SEC VIII Div. 1.
Vessel Dia OD = 610 mm
Vessel thickness = 12 mm
Design Pressure = 0.35 Mpa
Design Temperature = 148 C
Shell Length = 2500 mm
Top cover = 24" Standard WNRF flange
bottom head = 2:1 Ellipsoidal head (Nom. T = 14mm , Min. 12mm)
Client specified on data sheet that shell / head RT shall be 100%
Radiographed able joints
As per Figure UW-3
A = Longitudinal Seam (Butt weld)(single bevel) => 100% consider by client requirement but what will be exemption and requirement as per code..?? (please refer to specific clause)
B = Circumference seam (Butt weld) (Single bevel) => 100% consider by client requirement but what will be exemption and requirement as per code..?? (please refer to specific clause)
C = Nozzle Neck to Flange (Butt Weld) => What will be exemption and requirement criteria as per code.. ??(please refer to specific clause)
D = Shell chamber to Nozzle neck welding => What will be exemption and requirement criteria as per code.. ??(please refer to specific clause)
Thanking in advance!
Lets kill some confusion about the RT requirement in accordance with ASME SEC VIII Div. 1.
Vessel Dia OD = 610 mm
Vessel thickness = 12 mm
Design Pressure = 0.35 Mpa
Design Temperature = 148 C
Shell Length = 2500 mm
Top cover = 24" Standard WNRF flange
bottom head = 2:1 Ellipsoidal head (Nom. T = 14mm , Min. 12mm)
Client specified on data sheet that shell / head RT shall be 100%
Radiographed able joints
As per Figure UW-3
A = Longitudinal Seam (Butt weld)(single bevel) => 100% consider by client requirement but what will be exemption and requirement as per code..?? (please refer to specific clause)
B = Circumference seam (Butt weld) (Single bevel) => 100% consider by client requirement but what will be exemption and requirement as per code..?? (please refer to specific clause)
C = Nozzle Neck to Flange (Butt Weld) => What will be exemption and requirement criteria as per code.. ??(please refer to specific clause)
D = Shell chamber to Nozzle neck welding => What will be exemption and requirement criteria as per code.. ??(please refer to specific clause)
Thanking in advance!