Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

RT for welding pipe to flange

Status
Not open for further replies.

Mohamedhassanmido

Materials
Joined
Sep 3, 2013
Messages
24
Location
EG
Can I do RT test after welding pipe to flange 30 inch diameter? If yes what is the procedure and method?
 
Panoramic with "Rollpac" film - one shot, one film only required.
Cheers,
DD
 
what kind of weld?

Fillet as for a slip-on flange, butt weld?
 
racookpe,
How do you RT a fillet weld (especially on a slip on flange) ?
Regards,
DD
 
DekDee,
You would be surprised what some customers want; defies logic and the imagination.
 
DekDee - "How do you RT a fillet weld?"

That was the purpose of my question. But if it were a butt weld, he would be using a 30 inch dia RFWN, and I didn't want to make that assumption.
 
Are you working to a CODE? If you are strictly working to ASME Sec VIII D1 for a pressure vessel, then Refer to Fig UW-3 and UW-12. If you have a slip-on flange it is a Cat C and RT is not applicable (not required) even if the whole vessel calls out for a degree of examination. If you need to do RT (customer or service driven) then UT can probably be substituted, but you need to look at your situation if a slip-on would even be allowed.

 
racookpe,
My apologies.

weldstan,
Understood, thank you.

mohammedhassanmido,
I am lost for words !!! (I have a few but might get in trouble)
 
Slip-on flange should not require RT or UT because of the geometry being unfavourable to both. Surface crack detection (MPI for carbon steel, penetrant for stainless) shouls suffice.
 
If RT is not possible on a weld, you might want to check if TOFD (Time-of-Flight Diffraction) can help. This is a type of ultrasonic testing, but you can visualize the defects and also "around the corner".
 
OSIRIS7,
It is still a fillet weld (or two of them)- TOFD or manual UT is still pretty much useless on a fillet weld.
What are you actually looking for in your UT scan ?
Weldstan described it perfectly !
Regards,
DD
 
TOFD is an evolved UT. If I am correctly informed, you can look for defects in a fillet weld.
 
OSIRIS7,
Whereas slip on flanges are used in low pressure applications and the fillet welds are likely small, TOFD will not provide any valuable information.
 