As said above by weldtek , RT shall be done after PWHT for high alloy steels per UHA-33. This is because a delayed cracking or post heat treatment cracking may happened in or adjacent to welds after PWHT. This is not applicable to UCS steels. Common sense: you always need to do RT before PWHT to repair defects if any. Section VIII Div. 1 does not require RT after PWHT for carbon or low alloy steels.