Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

RT acceptence criteria

Status
Not open for further replies.

Tman1

Petroleum
Dec 5, 2012
25
Hy All

Can some one kindly explain to me on acceptance criteria for rounded indications...
ASME B31.3 refers us to ASME VIII appendix 4 which says under note (4) 1⁄16 in. for t greater than 2 in. (50 mm)
(c) Maximum Size of Rounded Indication. (See
Table 4-1 for examples.) The maximum permissible size
of any indication shall be 1⁄4t, or 5⁄32 in. (4 mm), whichever
is smaller.

is the table 4-1 supose to be used for maximum pore allowed?

we had an argument about this with the client.

Regards
 
Replies continue below

Recommended for you

Table 4-1 is to be used to determine the maximum pore size. It should be used in conjunction with the figures that follow to determine if your pores are to be considered scattered or isolated and with 4-3(d) to determine if they are to be considered aligned.
 
I would bring it in front of a experienced level II OR III with good equipment. I have been mistaken several times but resolved the issues with expert opinions.
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor