Hi All,
Following are the summary of two defects( Named as 7&7A) found in
one of our pipelines. As these two defects are 300mm apart under the defect interaction rule we can consider as one defect.(Named as 7 com.)
defect 7 ( Assessed defect length of 2.060Meter with an effective defect length of 1.340 Meter)
defect 7A ( Assessed defect length of 1.6 Meter with an effective defect length of 0.850 Meters)
If we consider pipe line design factor of 1.39, both defects need to be repaired under the RSTRENG mythology. Further as per the attached RSTRENG calculations show that when two defects combined together, effective length only pointing out to area where the defect 7 is. Combined defect effective length is smaller than if we consider the two defects separately. Appreciate if any one could explain this situation.
Following are the summary of two defects( Named as 7&7A) found in
one of our pipelines. As these two defects are 300mm apart under the defect interaction rule we can consider as one defect.(Named as 7 com.)
defect 7 ( Assessed defect length of 2.060Meter with an effective defect length of 1.340 Meter)
defect 7A ( Assessed defect length of 1.6 Meter with an effective defect length of 0.850 Meters)
If we consider pipe line design factor of 1.39, both defects need to be repaired under the RSTRENG mythology. Further as per the attached RSTRENG calculations show that when two defects combined together, effective length only pointing out to area where the defect 7 is. Combined defect effective length is smaller than if we consider the two defects separately. Appreciate if any one could explain this situation.