Hi All,

I'd like to know if there is a documented code, standard, or reference that I can use as a basis for the following formula that I found on the internet for calculating the dimensions of the reinforcing pad:

𝐿1=d+10𝑚𝑚
𝐿2=2d
𝑤=(𝐿2−𝐿1)/2
𝐶1= 𝐷_ℎ sin^(−1)⁡(d/𝐷 )(𝜋/180)+10𝑚𝑚
𝐶2=𝐶1+2𝑤

See the attachment for the photo.

I tried to search for references for the above formula, but nothing clearly states where it originated.

Thank you.

Regards,

marchieV
 
 https://files.engineering.com/getfile.aspx?folder=9373275c-b7ec-4721-9c23-d120704b7aea&file=Reinforcement-Pad-FORMULA.png
Replies continue below

Recommended for you

Your piping code will have the formula to use for branch connections.

So B31.3 is in section 304.3.4, but your dimensions don't seem to correspond.

"formula that I found on the internet "

Really needs no other comment....

At its most basic, the repad replaces the metal "lost" by the hole of the branch, usually within 1D of the hole, hence the L2 = 2x D

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
Hi LittleInch,

Thanks for the response.

I'm just wondering about the basis of the formula.
 
There's alittle bit more to it than that but when you look at the formula, it basically adds the metal taken away but excludes corrosion and other tolerances.