Hi All
Hope you all are enjoying your own day
i have one confusion related to acceptance criteria for rounded indication.
As given in section viii div 1 - page 419-4.3- ( f ) Regarding Rounded Indication Charts.
Rounded Indication Charts.
The rounded indications characterized as imperfections shall not exceed that shown in the charts. The charts in Figs. 4-3 through 4-8 illustrate various types of assorted, randomly dispersed and clustered rounded indications for different weld thicknesses greater than 1?8 in. (3 mm). These charts represent the maximum
acceptable concentration limits for rounded indications. The charts for each thickness range represent full-scale 6 in. (150 mm) radiographs, and shall not be enlarged or reduced. The distributions shown are not necessarily the patterns that may appear on the radiograph, but are typical of the concentration and size of indications permitted.
Questions are -
1- If indication ( rounded ) coming along the circumference ( full joint ) but concentration is less then as mention in chart , then its acceptable ?
2- Chart is for 6" film , so how we will judge in 12" in film , Is we need to check indication each 6" length?
Thanks and ton
With warm Regards,
Navin Kumar Tiwari
Hope you all are enjoying your own day

i have one confusion related to acceptance criteria for rounded indication.
As given in section viii div 1 - page 419-4.3- ( f ) Regarding Rounded Indication Charts.
Rounded Indication Charts.
The rounded indications characterized as imperfections shall not exceed that shown in the charts. The charts in Figs. 4-3 through 4-8 illustrate various types of assorted, randomly dispersed and clustered rounded indications for different weld thicknesses greater than 1?8 in. (3 mm). These charts represent the maximum
acceptable concentration limits for rounded indications. The charts for each thickness range represent full-scale 6 in. (150 mm) radiographs, and shall not be enlarged or reduced. The distributions shown are not necessarily the patterns that may appear on the radiograph, but are typical of the concentration and size of indications permitted.
Questions are -
1- If indication ( rounded ) coming along the circumference ( full joint ) but concentration is less then as mention in chart , then its acceptable ?
2- Chart is for 6" film , so how we will judge in 12" in film , Is we need to check indication each 6" length?
Thanks and ton
With warm Regards,
Navin Kumar Tiwari