May 31, 2001 #1 sylvester Mechanical Joined May 31, 2001 Messages 1 Location NL I am searching for the causes of this type of corrosion. Does anybody know information that leads me to an answer? Thanks in advance, Eric Voorneveld Project Leader/Engineer
I am searching for the causes of this type of corrosion. Does anybody know information that leads me to an answer? Thanks in advance, Eric Voorneveld Project Leader/Engineer
May 31, 2001 #2 rustbuster1 Materials Joined May 30, 2001 Messages 128 Location US You can get good information on this from arc_jmg@yahoo.com It involves a surface corrosion phenomenon on austenitic stainless steels - possibly ferritic and duplex grades too. Upvote 0 Downvote
You can get good information on this from arc_jmg@yahoo.com It involves a surface corrosion phenomenon on austenitic stainless steels - possibly ferritic and duplex grades too.
Aug 28, 2001 2 #3 corrosionlab Materials Joined Aug 28, 2001 Messages 2 Location US I suggest you visit the web site at http://www.corrosionlab.com/rouging/html Upvote 0 Downvote
Aug 28, 2001 #4 corrosionlab Materials Joined Aug 28, 2001 Messages 2 Location US Correrction to the last posting. Correct address is corrosionlab.com/rouging.html Upvote 0 Downvote