Roughness in pipe 1

Status
Not open for further replies.

SMIAH

Civil/Environmental
Jan 26, 2009
482
hello,

I would like to have the CHW, roughness (epsilon in Darcy Weibach) and Manning coefficient for a HDP pipe (ex.: Sclairpipe of KHW).

Initial guess would be:
CHW = 150
epsilon = 0.005 mm
n = 0.011

Thanks,
 