hirschaplin
Petroleum
Hello,
Have some problems with a roots blower. Twelve inch gears, 762 mm long bi-lobes. Horizontal gas flow.
Operating with a 80% hydrogen mixture.
Inlet about 0,6 barg / 30 deg C
Outlet about 1 barg / <70 deg C
Machine max. allowable speed as per the OEM is 1800 rpm.
The blower is driven by an electric motor with a VFD for speed control.
Normal vibration level RMS for 1100 rpm is around 3 mm/s. When we increased the rpm to 1350 the vibrations went up to 9,5 mm/s and then shortly suddenly went to 12,5 mm/s.
Currently operating at nitrogen for testing purpose, differential pressure at 400 mbar, 1000 rpm, vib RMS reading is around 4 mm/s.
Historical bearing RTD trends shows that there are sudden temperature spikes at bearings on the gear end. Temperature jumps from 80 deg C to 115 deg C very sudden.
The blower is balanced to g2.5 as per ISO 1940.
Aligned with proper laser tools.
There are NO vibrations on the foundation, or after the blower inlet/outlet expansion joints. No vibration levels means below 2 mm/s.
It seems like the machine is responding super bad to increasing the rpm above 1100 rpm. >1100 up until our max of around 1450 rpm works super bad with vibration levels at min 7.5 mm/s.
Problem is that the mechanical seals are leaking at high vibration levels. Need to maintain around 4 mm/s to have those seals leak free...
Any ideas?
Have some problems with a roots blower. Twelve inch gears, 762 mm long bi-lobes. Horizontal gas flow.
Operating with a 80% hydrogen mixture.
Inlet about 0,6 barg / 30 deg C
Outlet about 1 barg / <70 deg C
Machine max. allowable speed as per the OEM is 1800 rpm.
The blower is driven by an electric motor with a VFD for speed control.
Normal vibration level RMS for 1100 rpm is around 3 mm/s. When we increased the rpm to 1350 the vibrations went up to 9,5 mm/s and then shortly suddenly went to 12,5 mm/s.
Currently operating at nitrogen for testing purpose, differential pressure at 400 mbar, 1000 rpm, vib RMS reading is around 4 mm/s.
Historical bearing RTD trends shows that there are sudden temperature spikes at bearings on the gear end. Temperature jumps from 80 deg C to 115 deg C very sudden.
The blower is balanced to g2.5 as per ISO 1940.
Aligned with proper laser tools.
There are NO vibrations on the foundation, or after the blower inlet/outlet expansion joints. No vibration levels means below 2 mm/s.
It seems like the machine is responding super bad to increasing the rpm above 1100 rpm. >1100 up until our max of around 1450 rpm works super bad with vibration levels at min 7.5 mm/s.
Problem is that the mechanical seals are leaking at high vibration levels. Need to maintain around 4 mm/s to have those seals leak free...
Any ideas?